| Initial sealing temperature | Initial sealing temperature 51μm | Internal Method | 106 °C |
| Elmendorf tear strength | Elmendorf tear strength TD:51μm | ASTM D1922 | 1000 g |
| Elmendorf tear strength | Elmendorf tear strength MD:51μm | ASTM D1922 | 720 g |
| Dart impact | Dart impact 51μm | ASTM D1709B | >850 g |
| elongation | elongation TD:Break,51μm | ASTM D882 | 620 % |
| elongation | elongation MD:Break,51μm | ASTM D882 | 590 % |
| tensile strength | tensile strength TD:Break,51μm | ASTM D882 | 38.4 MPa |
| tensile strength | tensile strength MD:Break,51μm | ASTM D882 | 40.8 MPa |
| tensile strength | tensile strength TD:Yield,51μm | ASTM D882 | 11.0 MPa |
| tensile strength | tensile strength MD:Yield,51μm | ASTM D882 | 9.79 MPa |
| Secant modulus | Secant modulus 2%Secant,TD:51μm | ASTM D882 | 248 MPa |
| Secant modulus | Secant modulus 2%Secant,MD:51μm | ASTM D882 | 219 MPa |
| Thin film puncture strength | Thin film puncture strength 51μm | Internal Method | 11.0 J/cm³ |
| Thin film puncture strength | Thin film puncture strength 51μm | Internal Method | 71.2 N |
| Thin film puncture strength | Thin film puncture strength 51μm | Internal Method | 4.29 J |
| film thickness | film thickness | | 51 µm |