| Elmendorf tear strength | Elmendorf tear strength TD:25μm,Blown Film | ASTM D1922 | 440 g |
| Elmendorf tear strength | Elmendorf tear strength MD:25μm,Blown Film | ASTM D1922 | 230 g |
| Dart impact | Dart impact 25μm,Blown Film | ASTM D1709 | 600 g |
| elongation | elongation TD:Break,25μm,Blown Film | ASTM D882 | 560 % |
| elongation | elongation MD:Break,25μm,Blown Film | ASTM D882 | 450 % |
| tensile strength | tensile strength TD:Break,25μm,Blown Film | ASTM D882 | 45.9 MPa |
| tensile strength | tensile strength MD:Break,25μm,Blown Film | ASTM D882 | 57.2 MPa |
| tensile strength | tensile strength TD:Yield,25μm,Blown Film | ASTM D882 | 9.65 MPa |
| tensile strength | tensile strength MD:Yield,25μm,Blown Film | ASTM D882 | 12.8 MPa |
| Secant modulus | Secant modulus 1%Secant,TD:25μm,Blown Film | ASTM D882 | 188 MPa |
| Secant modulus | Secant modulus 1%Secant,MD:25μm,Blown Film | ASTM D882 | 165 MPa |
| film thickness | film thickness | | 25 µm |
| Initial sealing temperature | Initial sealing temperature 25μm,Blown Film | ASTMF88 | 102 °C |