Water vapor permeability | Water vapor permeability | ASTME96 | 12 g/m²/24hr |
Oxygen permeability | Oxygen permeability 铸造薄膜 | ASTM D3985 | 2800 cm³/m²/24hr |
Elmendorf tear strength | Elmendorf tear strength TD:铸造薄膜 | ASTM D1922 | 90 g |
Elmendorf tear strength | Elmendorf tear strength MD:铸造薄膜 | ASTM D1922 | 20 g |
Dart impact | Dart impact 铸造薄膜 | ASTM D1709 | 150 g |
elongation | elongation TD:Break,挤塑薄膜 | ASTM D882 | 700 % |
elongation | elongation MD:Break,挤塑薄膜 | ASTM D882 | 650 % |
tensile strength | tensile strength TD:Break,挤塑薄膜 | ASTM D882 | 37.9 MPa |
consumption | consumption | | 43.8 m²/kg |
tensile strength | tensile strength MD:Break,挤塑薄膜 | ASTM D882 | 44.8 MPa |
Secant modulus | Secant modulus TD:铸造薄膜 | ASTM D882 | 448 MPa |
Secant modulus | Secant modulus MD:铸造薄膜 | ASTM D882 | 483 MPa |
consumption | consumption | | 43.8 m²/kg |
Water vapor permeability | Water vapor permeability | ASTME96 | 12 g/m²/24hr |
Oxygen permeability | Oxygen permeability 铸造薄膜 | ASTM D3985 | 2800 cm³/m²/24hr |
Elmendorf tear strength | Elmendorf tear strength TD:铸造薄膜 | ASTM D1922 | 90 g |
Elmendorf tear strength | Elmendorf tear strength MD:铸造薄膜 | ASTM D1922 | 20 g |
Dart impact | Dart impact 铸造薄膜 | ASTM D1709 | 150 g |
Secant modulus | Secant modulus MD:铸造薄膜 | ASTM D882 | 483 MPa |
Secant modulus | Secant modulus TD:铸造薄膜 | ASTM D882 | 448 MPa |
tensile strength | tensile strength MD:Break,挤塑薄膜 | ASTM D882 | 44.8 MPa |
tensile strength | tensile strength TD:Break,挤塑薄膜 | ASTM D882 | 37.9 MPa |
elongation | elongation MD:Break,挤塑薄膜 | ASTM D882 | 650 % |
elongation | elongation TD:Break,挤塑薄膜 | ASTM D882 | 700 % |