film thickness | film thickness | | 20 µm |
Thin film puncture strength | Thin film puncture strength 20μm | Internal Method | 4.28 J |
Thin film puncture strength | Thin film puncture strength 20μm | Internal Method | 47.6 N |
Thin film puncture strength | Thin film puncture strength 20μm | Internal Method | 31.4 J/cm³ |
Secant modulus | Secant modulus 2%Secant,MD:20μm | ASTM D882 | 108 Mpa |
Initial sealing temperature | Initial sealing temperature 20μm | Internal Method | 93.9 °C |
Secant modulus | Secant modulus 2%Secant,TD:20μm | ASTM D882 | 115 Mpa |
tensile strength | tensile strength MD:Yield,20μm | ASTM D882 | 9.93 Mpa |
tensile strength | tensile strength TD:Yield,20μm | ASTM D882 | 5.45 Mpa |
tensile strength | tensile strength MD:Break,20μm | ASTM D882 | 44.6 Mpa |
tensile strength | tensile strength TD:Break,20μm | ASTM D882 | 29.8 Mpa |
elongation | elongation MD:Break,20μm | ASTM D882 | 350 % |
elongation | elongation TD:Break,20μm | ASTM D882 | 570 % |
Dart impact | Dart impact 20μm | ASTM D1709B | >830 g |
Elmendorf tear strength | Elmendorf tear strength MD:20μm | ASTM D1922 | 120 g |
Elmendorf tear strength | Elmendorf tear strength TD:20μm | ASTM D1922 | 410 g |