| tensile strength | tensile strength TD:Yield,51μm | ASTM D882 | 7.17 Mpa |
| tensile strength | tensile strength MD:Break,51μm | ASTM D882 | 45.4 Mpa |
| tensile strength | tensile strength TD:Break,51μm | ASTM D882 | 42.5 Mpa |
| elongation | elongation MD:Break,51μm | ASTM D882 | 590 % |
| elongation | elongation TD:Break,51μm | ASTM D882 | 630 % |
| Dart impact | Dart impact 51μm | ASTM D1709B | >830 g |
| Elmendorf tear strength | Elmendorf tear strength MD:51μm | ASTM D1922 | 560 g |
| Elmendorf tear strength | Elmendorf tear strength TD:51μm | ASTM D1922 | 730 g |
| Initial sealing temperature | Initial sealing temperature 51μm | Internal Method | 85.0 °C |
| Blocking force | Blocking force | ASTM D3354-89 | 70 g |
| film thickness | film thickness | | 51 µm |
| Thin film puncture strength | Thin film puncture strength 51μm | Internal Method | 8.09 J |
| Thin film puncture strength | Thin film puncture strength 51μm | Internal Method | 82.3 N |
| Thin film puncture strength | Thin film puncture strength 51μm | Internal Method | 21.9 J/cm³ |
| Secant modulus | Secant modulus 2%Secant,MD:51μm | ASTM D882 | 97.4 Mpa |
| Secant modulus | Secant modulus 2%Secant,TD:51μm | ASTM D882 | 96.9 Mpa |
| tensile strength | tensile strength MD:Yield,51μm | ASTM D882 | 8.07 Mpa |