| tensile strength | tensile strength TD:Break,51μm | ASTM D882 | 39.5 Mpa |
| elongation | elongation MD:Break,51μm | ASTM D882 | 690 % |
| elongation | elongation TD:Break,51μm | ASTM D882 | 700 % |
| tensile strength | tensile strength MD:Break,51μm | ASTM D882 | 50.3 Mpa |
| tensile strength | tensile strength TD:Yield,51μm | ASTM D882 | 6.34 Mpa |
| tensile strength | tensile strength MD:Yield,51μm | ASTM D882 | 5.79 Mpa |
| Secant modulus | Secant modulus 2%Secant,TD:51μm | ASTM D882 | 73.2 Mpa |
| Secant modulus | Secant modulus 2%Secant,MD:51μm | ASTM D882 | 72.8 Mpa |
| Thin film puncture strength | Thin film puncture strength 51μm | Internal Method | 20.3 J/cm³ |
| Thin film puncture strength | Thin film puncture strength 51μm | Internal Method | 83.6 N |
| Thin film puncture strength | Thin film puncture strength 51μm | Internal Method | 8.18 J |
| film thickness | film thickness | | 51 µm |
| Initial sealing temperature | Initial sealing temperature 51μm | Internal Method | 81.1 °C |
| Elmendorf tear strength | Elmendorf tear strength TD:51μm | ASTM D1922 | 620 g |
| Elmendorf tear strength | Elmendorf tear strength MD:51μm | ASTM D1922 | 470 g |
| Dart impact | Dart impact 51μm | ASTM D1709B | >850 g |