| Initial sealing temperature | Initial sealing temperature 51μm | Internal Method | 92.8 °C |
| Elmendorf tear strength | Elmendorf tear strength TD:51μm | ASTM D1922 | 840 g |
| Elmendorf tear strength | Elmendorf tear strength MD:51μm | ASTM D1922 | 560 g |
| Dart impact | Dart impact 51μm | ASTM D1709B | >830 g |
| elongation | elongation TD:Break,51μm | ASTM D882 | 580 % |
| elongation | elongation MD:Break,51μm | ASTM D882 | 620 % |
| tensile strength | tensile strength TD:Break,51μm | ASTM D882 | 45.4 Mpa |
| tensile strength | tensile strength MD:Break,51μm | ASTM D882 | 47.8 Mpa |
| tensile strength | tensile strength TD:Yield,51μm | ASTM D882 | 8.07 Mpa |
| tensile strength | tensile strength MD:Yield,51μm | ASTM D882 | 8.76 Mpa |
| Secant modulus | Secant modulus 2%Secant,TD:51μm | ASTM D882 | 123 Mpa |
| Secant modulus | Secant modulus 2%Secant,MD:51μm | ASTM D882 | 123 Mpa |
| Thin film puncture strength | Thin film puncture strength 51μm | Internal Method | 25.2 J/cm³ |
| Thin film puncture strength | Thin film puncture strength 51μm | Internal Method | 93.0 N |
| Thin film puncture strength | Thin film puncture strength 51μm | Internal Method | 9.16 J |
| film thickness | film thickness | | 51 µm |