So sánh vật liệu
Thông số kỹ thuật
| Basic Performance | Điều kiện kiểm tra | Phương pháp kiểm tra | HYOSUNG KOREA/B240P |
|---|---|---|---|
| melt mass-flow rate | 230℃,2.16Kg | ASTM D-1238 | 0.4 g/10min |
| density | ASTM D-792 | 0.91 |
| mechanical properties | Điều kiện kiểm tra | Phương pháp kiểm tra | HYOSUNG KOREA/B240P |
|---|---|---|---|
| Elongation at Break | ASTM D638/ISO 527 | 200 kg/cm²(MPa)[Lb/in²] | |
| Impact strength of cantilever beam gap | -20℃ | ASTM D-256 | 6 kg.cm/cm |
| Rockwell hardness | ASTM D785 | 90 | |
| Charpy Notched Impact Strength | ASTM D256/ISO 179 | 12 kg·cm/cm(J/M)ft·lb/in | |
| Impact strength of cantilever beam gap | 0℃ | ASTM D-256 | 10 kg.cm/cm |
| Elongation at Break | ASTM D-638 | 500 % | |
| tensile strength | 断点 | ASTM D-638 | 240 kg/cm |
| Yield点 | ASTM D-638 | 270 kg/cm | |
| Impact strength of cantilever beam gap | 23℃ | ASTM D-256 | 无破损 kg.cm/cm |
| Bending modulus | ASTM D-790 | 11500 kg/cm |
| thermal performance | Điều kiện kiểm tra | Phương pháp kiểm tra | HYOSUNG KOREA/B240P |
|---|---|---|---|
| Melting temperature | HS Method | 162 °C | |
| Vicat softening temperature | ASTM D-1525 | 150 °C | |
| Linear coefficient of thermal expansion | 0℃-110℃ | Dilatometor | 1.5×10 K |
| Physical properties | Điều kiện kiểm tra | Phương pháp kiểm tra | HYOSUNG KOREA/B240P |
|---|---|---|---|
| melt mass-flow rate | ASTM D1238/ISO 1133 | 0.4 g/10min |
| Electrical performance | Điều kiện kiểm tra | Phương pháp kiểm tra | HYOSUNG KOREA/B240P |
|---|---|---|---|
| Volume resistivity | HS Method | >10 Ω |