So sánh vật liệu
Thông số kỹ thuật
| mechanical properties | Điều kiện kiểm tra | Phương pháp kiểm tra | LX MMA KOREA/EG-920 |
|---|---|---|---|
| Impact strength of cantilever beam gap | Izod Notched | ASTM D-256 | 1.6 kg·cm/cm |
| bending strength | ASTM D-790 | 1.300 kg/cm | |
| Elongation at Break | ASTM D-638 | 3.5 % | |
| tensile strength | ASTM D-638 | 730 kg/cm | |
| Rockwell hardness | ASTM D-785 | 93 M-scale | |
| Bending modulus | ASTM D-790 | 33.000 kg/cm |
| thermal performance | Điều kiện kiểm tra | Phương pháp kiểm tra | LX MMA KOREA/EG-920 |
|---|---|---|---|
| specific heat | 0.35 cal/g/°C | ||
| Vicat softening temperature | 1kg | ASTM D-1525 | 100 °C |
| melt mass-flow rate | 230°C,3.8kg | ASTM D-1238 | 1.6 g/10min |
| Shrinkage rate | ASTM D995-51 | 0.2-0.6 % | |
| Hot deformation temperature | 18.56kg | ASTM D-648 | 96 °C |
| UL flame retardant rating | 1/8",1/16" | UL 94 | HB |
| Coefficient of sponge expansion | ASTM D-696 | 6×10 cm/cm/°C | |
| heat conduction | ASTM D-177 | 5×10 cal/seccm·°C/cm |
| Physical properties | Điều kiện kiểm tra | Phương pháp kiểm tra | LX MMA KOREA/EG-920 |
|---|---|---|---|
| density | ASTM D-792 | 1.18 | |
| transparency | 3.2mm | ASTM D-1003 | 93 % |
| Water absorption rate | 24h | ASTM D-570 | 0.3 % |
| reflectivity | ASTM D-542 | 1.49 |
| Electrical performance | Điều kiện kiểm tra | Phương pháp kiểm tra | LX MMA KOREA/EG-920 |
|---|---|---|---|
| Dielectric constant | 60Hz | ASTM D-150 | 4 |
| Dissipation factor | 60Hz | ASTM D-150 | 0.05 |
| Dielectric strength | 4KV/S | ASTM D-149 | 20 KV/mm |
| Volume resistivity | ASTM D-257 | >15 Ω.m |