So sánh vật liệu
Thông số kỹ thuật
| optical performance | Điều kiện kiểm tra | Phương pháp kiểm tra | Ester Industries Ltd./UmaPET HSCO |
|---|---|---|---|
| turbidity | 15.0μm | ASTM D1003 | 3.0 % |
| 12.0μm | ASTM D1003 | 3.0 % | |
| 25.0μm | ASTM D1003 | 4.0 % | |
| 20.0μm | ASTM D1003 | 3.5 % |
| mechanical properties | Điều kiện kiểm tra | Phương pháp kiểm tra | Ester Industries Ltd./UmaPET HSCO |
|---|---|---|---|
| Friction coefficient | Itself - Static6 | ASTM D1894 | 0.48 |
| Itself - Static5 | ASTM D1894 | 0.48 | |
| Itself - Dynamic1 | ASTM D1894 | 0.40 | |
| Itself - Dynamic3 | ASTM D1894 | 0.40 | |
| Itself - Dynamic2 | ASTM D1894 | 0.40 | |
| Itself - Static8 | ASTM D1894 | 0.48 | |
| Itself - Static7 | ASTM D1894 | 0.48 | |
| Itself - Dynamic4 | ASTM D1894 | 0.38 |
| Physical properties | Điều kiện kiểm tra | Phương pháp kiểm tra | Ester Industries Ltd./UmaPET HSCO |
|---|---|---|---|
| Shrinkage rate | MD:150°C,30分钟,0.0120mm | ASTM D1204 | 2.5 % |
| TD:150°C,30分钟,0.0250mm | ASTM D1204 | 0.40 % | |
| MD:150°C,30分钟,0.0250mm | ASTM D1204 | 2.0 % | |
| TD:150°C,30分钟,0.0120mm | ASTM D1204 | 0.40 % | |
| TD:150°C,30分钟,0.0150mm | ASTM D1204 | 0.40 % | |
| MD:150°C,30分钟,0.0150mm | ASTM D1204 | 2.5 % | |
| TD:150°C,30分钟,0.0200mm | ASTM D1204 | 0.40 % | |
| MD:150°C,30分钟,0.0200mm | ASTM D1204 | 2.0 % |
| film | Điều kiện kiểm tra | Phương pháp kiểm tra | Ester Industries Ltd./UmaPET HSCO |
|---|---|---|---|
| elongation | MD:Break,25μm | ASTM D882 | 100 % |
| tensile strength | MD:Break,15μm | ASTM D882 | 177 MPa |
| MD:Break,25μm | ASTM D882 | 172 MPa | |
| consumption | 12.0μm | Internal Method | 59.5 m²/kg |
| 25.0μm | Internal Method | 28.6 m²/kg | |
| elongation | MD:Break,15μm | ASTM D882 | 100 % |
| TD:Break,25μm | ASTM D882 | 90 % | |
| MD:Break,20μm | ASTM D882 | 100 % | |
| TD:Break,15μm | ASTM D882 | 90 % | |
| MD:Break,12μm | ASTM D882 | 100 % | |
| TD:Break,20μm | ASTM D882 | 90 % | |
| film thickness | 12.15.20.25µm | ||
| elongation | TD:Break,12μm | ASTM D882 | 90 % |
| tensile strength | TD:Break,15μm | ASTM D882 | 186 MPa |
| film thickness | 12152025 µm | ||
| consumption | 20.0μm | Internal Method | 35.7 m²/kg |
| tensile strength | MD:Break,12μm | ASTM D882 | 177 MPa |
| TD:Break,12μm | ASTM D882 | 186 MPa | |
| TD:Break,25μm | ASTM D882 | 181 MPa | |
| MD:Break,20μm | ASTM D882 | 172 MPa | |
| TD:Break,20μm | ASTM D882 | 181 MPa | |
| consumption | 15.0μm | Internal Method | 47.6 m²/kg |
| Supplementary Information | Điều kiện kiểm tra | Phương pháp kiểm tra | Ester Industries Ltd./UmaPET HSCO |
|---|---|---|---|
| wetting tension | Plainside:25.0μm | ASTM D2578 | 44 dyne/cm |
| Plainside:20.0μm | ASTM D2578 | 44 dyne/cm | |
| Plainside:12.0μm | ASTM D2578 | 44 dyne/cm | |
| Plainside:15.0μm | ASTM D2578 | 44 dyne/cm | |
| Coronaside:20.0μm | ASTM D2578 | 52 dyne/cm | |
| Coronaside:12.0μm | ASTM D2578 | 52 dyne/cm | |
| Coronaside:25.0μm | ASTM D2578 | 52 dyne/cm | |
| Coronaside:15.0μm | ASTM D2578 | 52 dyne/cm |