| impact performance | Điều kiện kiểm tra | Phương pháp kiểm tra | Altuglas International of Arkema Inc./VESTODUR® GF20 |
|---|---|---|---|
| Impact strength of simply supported beam without notch | -30°C,Complete Break | ISO 179/1eU | 65 kJ/m² |
| Charpy Notched Impact Strength | -30°C,Complete Break | ISO 179/1eA | 8.5 kJ/m² |
| 23°C,Complete Break | ISO 179/1eA | 9.0 kJ/m² | |
| Impact strength of simply supported beam without notch | 23°C,Complete Break | ISO 179/1eU | 60 kJ/m² |
| flammability | Điều kiện kiểm tra | Phương pháp kiểm tra | Altuglas International of Arkema Inc./VESTODUR® GF20 |
|---|---|---|---|
| Extreme Oxygen Index | ISO 4589-2 | 20 % | |
| Hot filament ignition temperature | 2.0mm | IEC 60695-2-13 | 800 °C |
| Flammability level | 1.6mm | IEC 60695-11-10,-20 | HB |
| 0.8mm | IEC 60695-11-10,-20 | HB | |
| Burning wire flammability index | 2.0mm | IEC 60695-2-12 | 750 °C |
| mechanical properties | Điều kiện kiểm tra | Phương pháp kiểm tra | Altuglas International of Arkema Inc./VESTODUR® GF20 |
|---|---|---|---|
| tensile strength | ISO 527-2/50 | 140 MPa | |
| Tensile modulus | ISO 527-2 | 7200 MPa | |
| Tensile strain | Break | ISO 527-2/50 | 3.5 % |
| thermal performance | Điều kiện kiểm tra | Phương pháp kiểm tra | Altuglas International of Arkema Inc./VESTODUR® GF20 |
|---|---|---|---|
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 220 °C |
| Vicat softening temperature | -- | ISO 306/B | 210 °C |
| Linear coefficient of thermal expansion | TD:23to55°C | ISO 11359-2 | 7E-05 cm/cm/°C |
| Melting temperature | ISO 11357-3 | 221to226 °C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 195 °C |
| Vicat softening temperature | -- | ISO 306/A | 220 °C |
| Linear coefficient of thermal expansion | MD:23to55°C | ISO 11359-2 | 6E-05 cm/cm/°C |
| Physical properties | Điều kiện kiểm tra | Phương pháp kiểm tra | Altuglas International of Arkema Inc./VESTODUR® GF20 |
|---|---|---|---|
| Shrinkage rate | MD | ISO 294-4 | 0.30 % |
| density | 23°C | ISO 1183 | 1.47 g/cm³ |
| Melt Volume Flow Rate (MVR) | 250°C/2.16kg | ISO 1133 | 16.0 cm³/10min |
| Water absorption rate | Saturation,23°C | ISO 62 | 0.45 % |
| Shrinkage rate | TD | ISO 294-4 | 1.5 % |
| Electrical performance | Điều kiện kiểm tra | Phương pháp kiểm tra | Altuglas International of Arkema Inc./VESTODUR® GF20 |
|---|---|---|---|
| Compared to the anti leakage trace index | --4 | IEC 60112 | PLC 2 |
| Dissipation factor | 23°C,100Hz | IEC 60250 | 3E-03 |
| Volume resistivity | 23°C | IEC 60093 | 1E+15 ohms·cm |
| Relative permittivity | 23°C,1MHz | IEC 60250 | 4.20 |
| Surface resistivity | IEC 60093 | 1E+13 ohms | |
| Dielectric strength | 1.00mm,in Oil | IEC 60243-1 | 27 kV/mm |
| Dissipation factor | 23°C,1MHz | IEC 60250 | 0.018 |
| Relative permittivity | 23°C,100Hz | IEC 60250 | 3.80 |
| Compared to the anti leakage trace index | SolutionA | IEC 60112 | PLC 2 |
| hardness | Điều kiện kiểm tra | Phương pháp kiểm tra | Altuglas International of Arkema Inc./VESTODUR® GF20 |
|---|---|---|---|
| Shore hardness | ShoreD | ISO 868 | 82 |
| Ball Pressure Test | ISO 2039-1 | 190 MPa |
| Supplementary Information | Điều kiện kiểm tra | Phương pháp kiểm tra | Altuglas International of Arkema Inc./VESTODUR® GF20 |
|---|---|---|---|
| Electrolytic corrosion | IEC 60426 | A1step |